| Eigentum | Einheit | Testmethode | Typische Werte | ||
| Dicke | Mikron | Intern | 15 | 20 | 25 |
| Zugfestigkeit Stärke TD | Mpa | ASTM-D-882 | 160 | 160 | 525 |
| Mpa | ASTM-D-882 | 280 | 280 | 420 | |
| Ultimative Dehnung MD TD | % | ASTM-D-882 | 160 | 160 | 600 |
| % | ASTM-D-882 | 60 | 60 | 695 | |
| Koeffizient Statisch | - | ASTM-D-1894 | 0, 35 | 0, 35 | 0, 35 |
| Heißsiegelfestigkeit | N/15mm | ASTM-D-2578 | 3 | 3 | 3 |
| Heißsiegeltemperatur | ºC | Intern | 116-132 | 116-132 | 116-132 |
| Dunst | % | ASTM-D-1003 | 1, 5 | 1, 5 | 1, 5 |
| WVTR | G /(m2•24 Std. ) 40 ºC | ASTM E 96 | 2, 2 | 2, 2 | 2, 2 |
| OTR | Ml /m2 •24 h•0, 1MPa | ASTM D 3985 | 40 | 40 | 40 |
| Aluminiumschicht | |||||
| Dicke | A | Intern | 300-500 | 300-500 | 300-500 |
| Gleichmäßigkeit | % | Intern | 96 | 96 | 96 |
| Bindungsfestigkeit | G/25mm | Intern | > 250 | > 250 | > 250 |